Pengaruh jumlah Cr2O3 terhadap kelemasan kulit atasan sepatu dari kulit biawak finish natural

Muchtar Lutfie, Widhiati Widhiati, Esti Rahayu

Abstract


The study is aimed at detecting the amount of Cr2O3 in percent added in the tanning of lizard skins for natural finished shoe upper leather. The materials used in this study are 36 pieces of dry preservated lizard skins which are tanned to natural finished shoe upper leather, while the tanning  agent used are Cr2O3 that added in veried amount as 0,5 %; 1,0 %; 1,5 % and 15 % Basyntan DLX. Using varian’s analysis, it is found that there is a significant difference in the softness of the leather caused by the amount of Cr2O3 added. The use of 1,5% Cr2O3 obviously shows the best result.

 

 

INTISARI

 

 

Penelitian ini bertujuan untuk mengetahui jumlah Cr2O3 (%) yang digunakan pada penyamakan kulit biawak untuk kulit atasan sepatu finish natural. Dengan menggunakan 36 lembar kulit biawak yang diawet kering diproses untuk kulit jadi untuk kulit atasan sepatu dengan finish natural. Bahan penyamak yang digunakan adalah Cr2O3 dengan variasi 0,5 %; 1,0 %, 1,5 % serta 15 % Basyntan DLX. Dengan menggunakan analisa varias’s ternyata didapatkan ada beda sangat nyata kelemasan akibat pengaruh perbedaan jumlah Cr2O3 yang diberikan. Penggunaan 1,5 % Cr2O3 adalah jumlah yang terbaik. 


Full Text:

PDF


DOI: http://dx.doi.org/10.20543/mkkp.v12i22.340

Refbacks

  • There are currently no refbacks.


Copyright (c) 1996 Muchtar Lutfie, Widhiati, Esti Rahayu

Creative Commons License
This work is licensed under a Creative Commons Attribution 4.0 International License.

 

MKKP indexed by:

Cover Page Cover Page     Cover Page    Cover Page     Cover Page     Cover Page     Cover Page     Cover Page     Cover Page     Cover Page    Cover Page    Cover Page    Cover Page     Cover Page     Cover Page   Cover Page   Cover Page   Cover Page   Cover Page              

 

 

 

Free counters!